LHGS04 de-oxygenation catalyst takes precious metal as active component basis loading on activated alumina carrier, which is mainly used to remove oxygen from hydrogen gas, also for nitrogen, CO, CO2, Argon and inert gas.
Operation for hydrogen gas and Argon gas could be done under normal temperature while space velocity (3~10)×103 h-1 and residual oxygen could be 0.2ppm. For synthesis gas, coal gas and coking dry gas, operation have to be done at temperature 110~140℃, pressure>0.1Mpa, space velocity (1~4)×103 h-1, and residual oxygen could be <1ppm.
Technology Properties
No
Test item
Technology parameter
Al2O3Compound Al2O3 size: Φ2-3 (mm)
Φ3-4 (mm)
Φ4-5 (mm)
1
Space velocity
(4-6) ×103 h-1
2
Optimal working temperature
-250℃ Normal temperature-250℃
De-oxygenation capacity
≥15ml. O2/g catalyst
3
Service life
≥ 3 years
O2 purifying ratio
≥ 95%
4
Bulk density
0.68±0.5 g/ml
5
Crushing strength
≥60N/pcs Φ2-3(mm)
6
Residual Oxygen
≤1.0 ppm
7
Humidity resistance
≤90%
8
Activity component
Pd, Pt
9
Appearance
Grey
10
Package
Moisture-proof and sealed
11
Suggested height/diameter
≥1:1
Contact person:Jane peng E-mail:jane@pxlihua.com
Skype:pxlihuajane
Tel:0086-799-6886893 Fax:0086-799-6835693 Mobile:0086-18979985936